Corrosion Resisting Alloy S129
Data
Sheet S129
Chemical
Composition Limits
|
Weight
% |
C |
Si
|
Mn |
P+S max |
Cr |
Mo |
Ni
|
Others |
S129 |
0.12 max |
0.20/1.00 |
0.50/2.00 |
0.035P 0.025S
|
17.00/19.00 |
- |
8.00/11.00 |
Ti5XC min |
2S129 |
0.08 max |
0.20/1.00 |
0.50/2.00 |
0.035P 0.025S
|
17.00/19.00 |
0.070 max |
8.00/11.00 |
Ti5XC/0.80 |
Chemically similar
British Specifications BS.970
Pt4.
|
Weight
% |
C |
Si
|
Mn |
P+S max |
Cr |
Mo |
Ni
|
Others |
321S20
321S12
(EN58 B/C)
|
0.12 max |
0.20/1.00 |
0.50/2.00 |
0.045P 0.030S
|
17.00/19.00 |
- |
8.00/11.00 |
5XC / 0.90 (Ti) |
Other Chemically
similar Specifications |
Weight
% |
C |
Si
|
Mn |
P+S max |
Cr |
Mo |
Ni |
Others |
AFNOR
Z10CNT 18-11
Z6CNT18-11
|
0.12 max |
1.00 max |
2.00 max |
0.040P 0.030S
|
17.00/19.00 |
- |
10.00/12.00 |
Ti5XC/0.80 |
AISI
321/
SAE 30321
|
0.80 max |
1.00 max |
2.00 max |
0.045P
0.030S
|
17.00/19.00 |
- |
9.00/ 12.00 |
Ti 5XC/min
|
AMS
5645
|
0.80 max |
1.00 max |
2.00 max |
0.040P
0.030S
|
17.00/19.00 |
0.75 max |
8.00/ 12.00 |
Ti 6XC/0.70
Cu 0.050 max
|
MIL-S-862B
321 |
0.80 max |
1.00 max |
2.00 max |
0.045P
0.030S
|
17.00/ 19.00 |
- |
9.00/ 12.00 |
Ti 5XC
|
MIL-S-27419
321 |
0.80 max |
1.00 max |
2.00 max |
0.025
|
17.00/20.00 |
- |
9.00/ 13.00 |
Ti 0.75max
Cu 0.70max
|
WS 1.4541 X10CrNiTi18 9 |
1.00 max |
1.00 max |
2.00 max |
0.045P
0.030S
|
17.00/ 19.00 |
- |
9.00/ 11.50 |
Ti 5XCmin
|
Austenitic
Steel |
EN |
AISI |
UNS |
International
names |
Usual
names |
Standards
or Specifications |
1.4541 |
321 |
S32100 |
GB: S129 |
Z10CNT18-10
Z6CNT18-10
X6CrNiTi18
|
AIR
9160 C
DMD
276-22
AMS-QQS763
321
ASNA3202
ASNA3139
BLFG248101
AMS5645
BLFE248101 |
prEN
3487
CR
1.3.0.5
DMD
0276-22
GAM
MM02
SM16602
prEN
2462
LA
31
LA
297
|
General characteristics
Core 321/4541 is a titanium-stabilized austenitic stainless steel with improved intergranular corrosion resistance
for an extended temperature range. 321 / EN 1.4541 is an austenitic stainless steel that belongs to the standard
CrNi stainless steel family. 321 / EN 1.4541 can be welded without becoming susceptible to intergranular corrosion.
The austenitic CrNi standard grades are the most widely used group of stainless steels.
Their well-balanced material properties make them suitable for the fabrication of many products.
Due to its titanium content, 321 / EN 1.4541 can be used at elevated temperatures.
For high-temperature applications, the use of the optimised high-temperature 321H / EN 1.4878 is recommended.
321 / EN 1.4541 is available in many product forms and dimensions,
Polishing of 321 / EN 1.4541 is limited due to its titanium alloying.
Typical applications
Annealing covers
Stack liners
Automotive exhaust systems
Welded pressure vessels
Flanges and valves
Disclaimer
Every effort is made to ensure that
technical specifications are accurate. However, technical specifications
included herein should be used as a guideline only. All specifications are
subject to change without notice.
|