ALLOY 47 / 50 TYPICAL
NOMINAL CHEMISTRY |
|
ALLOY 47 / 50 TYPICAL
TENSILE STRENGTH |
|
|
| NICKEL (NI) |
48.0 |
ANNEALED |
85,000 MAX. |
| CHROMIUM (CR) |
0.10 |
1/4 HARD |
90,000 to 115,000 |
| MANGANESE (MN) |
0.80 |
1/2 HARD |
105,000 to 125,000 |
| SILICON (SI) |
0.30 |
HARD |
120,000 MIN. |
| CARBON (C) |
0.05 |
|
| ALUMINUM (AL) |
0.10 |
TYPICAL HARDNESS,
ROCKWELL B |
| MAGNESIUM (MG) |
0.50 |
ANNEALED |
70 MAX. |
| ZIRCONIUM (ZR) |
0.00 |
1/4 HARD |
78 to 83 |
| TITANIUM (TI) |
0.00 |
1/2 HARD |
84 to 88 |
| PHOSPHORUS (P) |
0.025 |
|
|
| SULFUR (S) |
0.025 |
|
|
| IRON |
BALANCE |
|
|
| |
TYPICAL
LINEAR COEFFICIENT OF THERMAL EXPANSION
(cm. per cm. C x 10 - 6) |
30 to 100 |
9.4 |
| 30 to 200 |
9.4 |
| 30 to 300 |
8.8 |
| 30 to 350 |
9.0 |
| 30 to 400 |
8.7 |
| 30 to 425 |
8.9 |
| 30 to 450 |
9.0 |
| 30 to 500 |
9.4 |
| 30 to 550 |
10.2 |
| 30 to 600 |
10.4 |
| 30 to 700 |
11.3 |
| 30 to 800 |
12.1 |
| 30 to 900 |
13.0 |
| 30 to 1000 |
13.9 |
| |
* PLEASE NOTE THIS IS A NOMINAL DATA SHEET
Top of Page
Disclaimer
Every
effort is made to ensure that technical specifications are accurate.
However, technical specifications included herein should be used as a
guideline only. All specifications are subject to change without notice.
|