Request
for Quotation
NOMINAL DATA SHEET
ALLOY 52 TYPICAL
NOMINAL CHEMISTRY |
|
ALLOY 52 TYPICAL
TENSILE STRENGTH |
|
|
NICKEL (NI) |
50.5 |
ANNEALED |
85,000 MAX. |
CHROMIUM (CR) |
0.10 |
1/4 HARD |
90,000 to 115,000 |
MANGANESE(MN) |
0.60 |
1/2 HARD |
105,000 to 125,000 |
SILICON (SI) |
0.30 |
HARD |
120,000 MIN. |
CARBON (C) |
0.05 |
|
ALUMINUM (AL) |
0.10 |
TYPICAL HARDNESS,
ROCKWELL B |
MAGNESIUM (MG) |
0.50 |
ANNEALED |
70 MAX. |
ZIRCONIUM (ZR) |
0.00 |
1/4 HARD |
78 to 83 |
TITANIUM (TI) |
0.00 |
1/2 HARD |
84 to 88 |
PHOSPHORUS (P) |
0.025 |
|
|
SULFUR (S) |
0.025 |
|
|
IRON |
BALANCE |
|
|
|
TYPICAL
LINEAR COEFFICIENT OF THERMAL EXPANSION
(cm. per cm. C x 10 - 6)
|
30 to 100 |
10.5 |
30 to 200 |
10.4 |
30 to 300 |
10.2 |
30 to 350 |
10.2 |
30 to 400 |
10.1 |
30 to 425 |
N/A |
30 to 450 |
10.1 |
30 to 500 |
10.0 |
30 to 550 |
10.5 |
30 to 600 |
10.8 |
30 to 700 |
11.7 |
30 to 800 |
12.5 |
30 to 900 |
13.3 |
30 to 1000 |
14.2 |
|
* PLEASE NOTE THIS IS A NOMINAL DATA SHEET
Top of Page
Disclaimer
Every
effort is made to ensure that technical specifications are accurate.
However, technical specifications included herein should be used as a
guideline only. All specifications are subject to change without notice.
|